As to the most effective mesh for the screen or grating no definite
rule can be given, as that depends so largely on the size of the gold
particles contained in the gangue. The finer the particles the closer
must be the mesh, and nothing but careful experiment will enable the
battery manager to decide this most important point. The American
slotted screens are best; they wear better than the punched gratings and
can be used of finer gauge. Woven steel wire gauze is employed with good
effect in some mills where especially fine trituration is required. This
class of screen requires special care as it is somewhat fragile, but
with intelligent treatment does good work.
The fall or inclination of the tables, both copper and blanket strakes,
is also regulated by the class of ore. If it should be heavy then the
fall must be steeper. A fair average drop is 3/4 inch to the foot. Be
careful that your copper tables are thoroughly water-tight, for remember
you are dealing with a very volatile metal, quicksilver; and where water
will percolate mercury will penetrate.
The blanket tables are simply a continuation of the mercury tables, but
covered with strips of coarse blanket, green baize, or other flocculent
material, intended to arrest the heavier metallic particles which, owing
to their refractory nature, have not been amalgamated.
The blanket table is, however, a very unsatisfactory concentrator
at best, and is giving place to mechanical concentrators of various
descriptions.
An ancient Egyptian gold washing table was used by the Egyptians in
treating the gold ores of Lower Egypt. The ore was first ground, it is
likely by means of some description of stone arrasts and then passed
over the sloping table with water, the gold being retained in the
riffles. In these the material would probably be mechanically agitated.
Although for its era ingenious it will be plain to practical men that if
the gold were fine the process would be very ineffective. Possibly, but
of this I have no evidence, mercury was used to retain the gold on the
riffles, as previously stated. This method of saving the precious metal
was known to the ancients.
At a mine of which I was managing director the lode was almost entirely
composed of sulphide of iron, carbonate of lime or calcspar, with a
little silica. In this case it has been found best to crush without
mercury, then run the pulp into pans, where it is concentrated. The
concentrates are calcined in a common reverberatory furnace, and
afterwards amalgamated with mercury in a special pan, the results as to
the proportion of gold extracted being very satisfactory; but it does
not therefore follow that this process would be the most suitable in
another mine where the lode stuff, though in some respects similar, yet
had points of difference.
Public-domain text, read in full here on John Shaqi.
Reviews
Reviews
No reviews yet
Be the first to share your thoughts on this work.
Elsewhere in the archive
Join the Discussion
Join the discussion
Sign in to leave a comment or review.
Sign InorCreate an account