_To find the Actual Horse-power_ of an engine, multiply the area of the
cylinder in square inches by the average effective pressure in pounds
per square inch, less 3 lb. per square inch as the frictional allowance,
and also by the speed of the piston in feet per minute, dividing the
product by 33,000, and the quotient will be the actual horse-power.
“SCALING” COPPER PLATES.
To “scale” copper plates they may be put over a charcoal or coke fire to
slowly sublimate the quicksilver. Where possible, the fireplace of a
spare boiler can be utilised, using a thin red fire. After the entire
evaporation of the quicksilver the plates should be slowly cooled,
rubbed with hydrochloric acid, and put in a damp place overnight, then
rubbed with a solution of sal ammoniac and nitre in equal parts, and
again heated slowly over a red fire. They must not be allowed to get red
hot; the proper degree of heat is indicated by the gold scale rising in
blisters, when the plates are to be taken from the fire and the gold
scraped off. Any part of the plate on which the gold has not blistered
should be again rubbed with the solution and fired. The gold scale
should be collected in a glass or earthen dish and covered with nitric
acid, till all the copper is dissolved, when the gold can be smelted in
the usual way; but when it is molten, corrosive sublimate should be put
in the crucible till a blue flame ceases to be given off.
_A Second Method._
The simplest plan I know is to have a hole dug nine inches deep by about
the size of the plate to be scaled; place a brick at each corner, and on
each side, halfway between. Get up a good fire, and let it burn down to
strong embers, or use charcoal, then place the plate on three bars of
iron extending between the three pairs of bricks, have a strong solution
of borax ready in which soak strips of old “table blanket,” laying these
over the plate and sprinkling them with the borax solution when the
plate gets too hot. After a time the deposit of mercury and gold on the
plate will assume a white, efflorescent appearance, and may then be
readily parted from the copper.
_Another Method._
Heat the plate over an open fire, to drive off the mercury; after which,
let it cool, and saturate with dilute sulphuric acid for three hours, or
longer; then sprinkle over the surface a mixture of equal parts of
common salt and sal ammoniac, and heat to redness. When cool, the gold
scale comes off freely; the scale is then boiled in nitric or sulphuric
acid, to remove the copper, previous to melting. Plates may be scaled
about once in six months, and will under ordinary circumstances produce
about one ounce of clean gold for each superficial foot of copper
surface employed. I always paint the back of the plate with a mixture of
boiled oil and turpentine, or beeswax dissolved in turpentine, to
prevent the acid attacking the copper.
HOW TO SUPPLY MERCURY TO MORTAR BOXES.
Public-domain text, read in full here on John Shaqi.
Reviews
Reviews
No reviews yet
Be the first to share your thoughts on this work.
Elsewhere in the archive
Join the Discussion
Join the discussion
Sign in to leave a comment or review.
Sign InorCreate an account