Getting Gold: A Practical Treatise for Prospectors, Miners and StudentsJohnson, J. C. F. (Joseph Colin Francis)
History
Getting Gold: A Practical Treatise for Prospectors, Miners and Students
Johnson, J. C. F. (Joseph Colin Francis)
Gold mines and mining
With inadequate material and appliances to hand, the following will
be found easier to construct and more lasting when constructed. Only
a single piece of iron is required, and, at a pinch, one could even
dispense with that by using a slab of talcose material, roughly shaping
a hearth therein and making a hole for the blast. First, construct a
framing about the height of an ordinary smith's forge. This can made
with saplings and bark, or better still, if available, out of an empty
packing case about three feet square. Fill the frame or case with
slightly damped earth and ram it tight, leaving the usual hollow hearth.
Then form a chamber below the perforated hearth opening to the rear.
Now construct a centrifugal fan, such as is used for the ventilation of
shallow shafts and workings. Set this up behind the hearth and revolve
by means of a wooden multiplying wheel. A piece of ordinary washing line
rope, or sash line rope, well resined if resin can be got--but pitch,
tar, or wax will do by adding a little fine dust to prevent sticking--is
used as a belt. With very rough materials a handy man can thus make a
forge that will answer ordinary requirements.--N.B. Do not use clay for
your hearth bed unless you can get a highly aluminous clay, and can give
it full time to dry before the forge fire is lit. Ordinary surface soil,
not too sandy, acts well, if damped and rammed thoroughly. Of course,
if you can get an iron nozzle for your blower the whole operation is
simplified.
SIMPLE WAY OF MAKING CHARCOAL
Dig a pit 5 feet square by 3 feet deep and fill with fuel. After
lighting, see that the pit is kept full. The hot embers will gradually
sink to the bottom. The fuel should be kept burning fiercely until the
pit seems almost full, when more fuel should be added, raising the heap
about a foot above the level of the ground. The earth dug out of the pit
should then be shovelled back over the burning mass. After leaving it to
cool for 24 hours the pit will be found nearly full of charcoal. About
one-quarter the weight of the dry fuel used should be recovered in
charcoal.
ROUGH SMELTING ON THE MINE
Rough smelting on the mine is effected with a flux of borax, carbonate
of soda, or, as I have often done, with some powdered white glass. When
the gold is smelted and the flux has settled down quietly in a liquid
state, the bulk of the latter may be removed, to facilitate pouring into
the mould, by dipping an iron rod alternately into the flux and then
into a little water, and knocking off the ball of congealed flux which
adheres after each dip. This flux should, however, be crushed with a
pestle and mortar and panned off, as, in certain cases, it may contain
tiny globules of gold.
MISFIRES IN BLASTING
Public-domain text, read in full here on John Shaqi.
Reviews
Reviews
No reviews yet
Be the first to share your thoughts on this work.
Elsewhere in the archive
Join the Discussion
Join the discussion
Sign in to leave a comment or review.
Sign InorCreate an account