Scientific American Supplement, No. 508, September 26, 1885Various
Science
Scientific American Supplement, No. 508, September 26, 1885
Various
Science -- Periodicals
From what precedes, it will be seen that the outlet is entirely
closed, so that, in order that the water may escape, it must pass into
the pipe in the direction, E D B A C.
This granted, let us see how the apparatus works: In measure as the
water rises in the reservoir, the siphon gradually loses weight, and
its extremity, B D H, is finally lifted by the thrust, so that the
entire affair revolves upon the studs, K, until the chain becomes
taut. The apparatus then ceases to rise; but the water, ever
continuing to rise, finally reaches the apex, _b_, of the smaller
siphon, and, through it, enters the air chamber and fills it. The
equilibrium being thus broken, the siphon descends to the bottom,
becomes primed, and empties the reservoir. When the level of the
water, in descending, is at the height of the small siphon, _a b c_,
this latter, which is also primed, empties the chamber, F, in turn, so
that, at the moment the large siphon loses its priming, the entire
apparatus is in the same state that it was at first.
In short, when the water enters the reservoir, the siphon, movable
upon its base, rises to the height at which it is desired that the
flow shall take place. Being arrested at this point by the chain, it
becomes primed, and sinks, and the water escapes. When the water is
exhausted, the siphon rises anew in order to again sink; and this goes
on as long as the period of irrigation lasts.
This apparatus, which is simple in its operation, and not very costly,
is being employed with success for irrigating several meadows in the
upper basin of the Allier.--_Le Genie Civil._
* * * * *
ASSAY OF EARTHENWARE GLAZE.
Lead oxide melted or incompletely vitrified is still in common use in
the manufacture of inferior earthenware, and sometimes leads to
serious results. To detect lead in a glaze, M. Herbelin moistens a
slip of white linen or cotton, free from starch, with nitric acid at
10 per cent. and rubs it for ten to fifteen seconds on the side of the
utensil under examination, and then deposits a drop of a solution of
potassium iodide, at 5 per cent. on the part which has been in
contact. A lead glaze simply fused gives a very highly colored yellow
spot of potassium iodide; a lead glaze incompletely vitrified gives
spots the more decided, the less perfect the vitrification; and a
glaze of good quality gives no sensible color at all.--_M. Herbelin._
* * * * *
ON THE ELECTRICAL FURNACE AND THE REDUCTION OF THE OXIDES OF BORON,
SILICON, ALUMINUM, AND OTHER METALS BY CARBON.[1]
[Footnote 1: Read at the recent meeting of the American
Association, Ann Arbor, Mich.]
By EUGENE H. COWLES, ALFRED H. COWLES, AND CHARLES F. MABERY.
Public-domain text, read in full here on John Shaqi.
Reviews
Reviews
No reviews yet
Be the first to share your thoughts on this work.
Elsewhere in the archive
Join the Discussion
Join the discussion
Sign in to leave a comment or review.
Sign InorCreate an account