An important property rendering drying of wood peculiarly difficult is
the changes which occur in the hygroscopic properties of the surface
of a stick, and the rate at which it will allow moisture to pass
through it. If wood is dried rapidly the surface soon reaches a
condition where the transfusion is greatly hindered and sometimes
appears almost to cease. The nature of this action is not well
understood and it differs greatly in different species. Bald cypress
(_Taxodium distichum_) is an example in which this property is
particularly troublesome. The difficulty can be overcome by regulating
the humidity during the drying operation. It is one of the factors
entering into production of what is called "case-hardening" of wood,
where the surface of the piece becomes hardened in a stretched or
expanded condition, and subsequent shrinkage of the interior causes
"honeycombing," "hollow-horning," or internal checking. The outer
surface of the wood appears to undergo a chemical change in the nature
of hydrolization or oxidization, which alters the rate of absorption
and evaporation in the air.
As the total amount of shrinkage varies with the rate at which the
wood is dried, it follows that the outer surface of a rapidly dried
board shrinks less than the interior. This sets up an internal stress,
which, if the board be afterward resawed into two thinner boards by
slicing it through the middle, causes the two halves to cup with their
convex surfaces outward. This effect may occur even though the
moisture distribution in the board has reached a uniform condition,
and the board is thoroughly dry before it is resawed. It is distinct
from the well-known "case-hardening" effect spoken of above, which is
caused by unequal moisture conditions.
The manner in which the water passes from the interior of a piece of
wood to its surface has not as yet been fully determined, although it
is one of the most important factors which influence drying. This must
involve a transfusion of moisture through the cell walls, since, as
already mentioned, except for the open vessels in the hardwoods, free
resin ducts in the softwoods, and possibly the intercellular spaces,
the cells of green wood are enclosed by membranes and the water must
pass through the walls or the membranes of the pits. Heat appears to
increase this transfusion, but experimental data are lacking.
It is evident that to dry wood properly a great many factors must be
taken into consideration aside from the mere evaporation of moisture.
Losses Due to Improper Kiln-drying
In some cases there is practically no loss in drying, but more often
it ranges from 1 to 3 per cent, and 7 to 10 per cent in refractory
woods such as gum. In exceptional instances the losses are as high as
33 per cent.
In air-drying there is little or no control over the process; it may
take place too rapidly on some days and too slowly on others, and it
may be very non-uniform.
Public-domain text, read in full here on John Shaqi.
Reviews
Reviews
No reviews yet
Be the first to share your thoughts on this work.
Elsewhere in the archive
Join the Discussion
Join the discussion
Sign in to leave a comment or review.
Sign InorCreate an account