The Boot and Shoe Manufacturers' Assistant and Guide.: Containing a Brief History of the Trade. History of India-rubber and Gutta-percha, and Their Application to the Manufacture of Boots and Shoes. Full Instructions in the Art, With Diagrams and Scales, Etc., Etc. Vulcanization and Sulphurization, English and American Patents. With an Elaborate Treatise on Tanning.
History
The Boot and Shoe Manufacturers' Assistant and Guide.: Containing a Brief History of the Trade. History of India-rubber and Gutta-percha, and Their Application to the Manufacture of Boots and Shoes. Full Instructions in the Art, With Diagrams and Scales, Etc., Etc. Vulcanization and Sulphurization, English and American Patents. With an Elaborate Treatise on Tanning.
Footwear industry; Gutta-percha; Rubber; Tanning
The following are good average proportions: about three parts caoutchouc
for every six parts of gutta-percha, or one part of sulphur for every
eight parts of gutta-percha, or two parts of caoutchouc, and one part of
sulphur for every six parts of gutta-percha. When caoutchouc, however,
is employed to increase the elasticity of the gutta-percha, a degree of
heat, of not less than 150° Fahrenheit is necessary to effect the
amalgamation of the two substances. The caoutchouc is most conveniently
introduced into the machine at the same time with the gutta-percha, but
the sulphur should be dropped into and upon the gutta percha from time
to time, and in small quantities at a time. The gutta-percha takes up
the other materials readily, and the whole are, at the end of the
process, thoroughly amalgamated. Should it be desired to give any color
to the mass, the requisite pigment or coloring matter is introduced in
the same manner as the sulphur, and also in small quantities at a time.
The coloring matter penetrates every part of the mass, and becomes
perfectly amalgamated and identified with it. The gutta-percha may be
also improved in smoothness, by incorporating with it some pulverized
French or Turkey chalk, or other soft powder, adding it in same way as
the sulphur, or should it be desired to make it rough, and abrasive, it
may be mixed up with some ground emery, sand, or other hard substance,
in a granular state.
* * * * *
There are other combinations in which the gutta-percha in its plastic
state, intimately mixed or blended with other materials, as for
example:—There may be added to the gutta-percha, while in the kneading
machine, paper pulp, wood dust, leather dust, hair bristles, oakum, &c.
(taking care when they are not in a comminuted state, to cut them up
small) and compound fabrics will be thus produced very suitable for
paring, roofing, sheathing, and other purposes.
APPLICATIONS IN STATE OF SOLUTION.
As before stated the gutta-percha may be dissolved in most of the
essential oils, and by the application of a gentle heat, the patentee
states that he prefers using for the purpose, rectified naptha, or
rectified oil of turpentine. It may also be applied in a state of
solution to rendering water and air proof, or cementing the various
articles to which gutta-percha has been before stated to be applicable
for these purposes in a plastic state, when sulphur imposed upon or
between the surfaces of articles. It may be applied in this fluid state,
to the saturation of cordage of all sorts, in order to increase its
strength, and render it water proof, and as a size for stiffening silks,
ribbons, and other fabrics. And lastly, it may be employed in this
liquid state mixed with colors, for printing silk, cotton, leather, and
other fabrics.
R. A. BROOMAN caused another patent to be issued, under date of March
27, 1845.
Public-domain text, read in full here on John Shaqi.
Reviews
Reviews
No reviews yet
Be the first to share your thoughts on this work.
Elsewhere in the archive
Join the Discussion
Join the discussion
Sign in to leave a comment or review.
Sign InorCreate an account