The Boot and Shoe Manufacturers' Assistant and Guide.: Containing a Brief History of the Trade. History of India-rubber and Gutta-percha, and Their Application to the Manufacture of Boots and Shoes. Full Instructions in the Art, With Diagrams and Scales, Etc., Etc. Vulcanization and Sulphurization, English and American Patents. With an Elaborate Treatise on Tanning.
History
The Boot and Shoe Manufacturers' Assistant and Guide.: Containing a Brief History of the Trade. History of India-rubber and Gutta-percha, and Their Application to the Manufacture of Boots and Shoes. Full Instructions in the Art, With Diagrams and Scales, Etc., Etc. Vulcanization and Sulphurization, English and American Patents. With an Elaborate Treatise on Tanning.
Footwear industry; Gutta-percha; Rubber; Tanning
A VARNISH WITH WHICH COLORS MAY BE MIXED, AND VERY SUITABLE FOR COATING
ARTICLES IN GUTTA-PERCHA.—Take 100 lbs. gutta-percha, 18 lbs. 12 oz. gum
opal, 50 lbs. linseed oil, 200 lbs. spirits of turpentine, and mix the
whole together.
A VARNISH FOR UNPAINTED ARTICLES IN ROUGH WOOD.—Take 50 lbs.
India-rubber, 100 lbs. gutta-percha, 30 lbs. gum opal, 70 lbs. gum
damar, 150 lbs. linseed oil, 75 lbs. sugar of lead, 500 lbs. spirits of
turpentine.
A VARNISH FOR ARTICLES OF METAL.—Take 100 lbs. gutta-percha, 20 lbs. gum
opal, 75 lbs. linseed oil, 25 lbs. sugar of lead, 200 lbs. spirits of
turpentine.
W. JOHNSON. Improvements in the treatment, preparation, or manufacture
of sheet caoutchouc, and in the combination thereof with cloth and other
fabrics. (A communication.) Dated October 3, 1856.
This relates to a mode of preparing sheets of caoutchouc, and combining
them firmly with cloth and other fabrics, to produce goods for the
manufacture of articles of various degrees of elasticity, and consists
in preparing sheets of vulcanized caoutchouc, by desulphurizing their
surfaces by first boiling the sheets in caustic alkali, and afterwards
in salt pickle, to neutralize the alkali remaining on the sheet, and
then washing the same. These sheets are then roughed on their surfaces,
and the fabric to which they are to be applied is prepared by coating
the surfaces thinly with a solution of caoutchouc dissolved in some
solvent, and then thoroughly evaporating the solvent.
F. C. JEUNE. An improved manufacture of floor cloth. Dated May 26, 1856.
The patentee mixes in a masticating machine, India-rubber, (partly the
waste of vulcanized rubber) and gutta percha, to produce a binding
substance, and throws in ground cedar wood, or other vegetable dust, for
increasing the bulk, and reducing the cost. When the mixing is effected,
he adds fibrous substances in length, to impart toughness, and rolls the
compound between rollers into sheets, which he submits to steam or hot
air, to complete the adhesion of the particles.
C. GOODYEAR. An improvement in combining gutta-percha and asphalt or
pitch. Dated August 30, 1856.
This consists in combining gutta-percha with asphalt or pitch, by the
aid of hot water. They are, when desired, further combined with sulphur,
with India-rubber, or other matters; and compounds are, when required,
subjected to high temperature.
A. LORIMIER. An improvement in re-working vulcanized India-rubber. Dated
October 20, 1856.
This consists in preparing the waste of vulcanized India-rubber by
crushing the same between pressing rollers, then subjecting it to a
considerable degree of heat, and whilst so heated causing it to be
stirred, by which means the mass is progressively brought into a fluid
state. It is then allowed to cool, but before becoming cold, a solvent
of India-rubber is added, by which an India-rubber cement is produced.
Public-domain text, read in full here on John Shaqi.
Reviews
Reviews
No reviews yet
Be the first to share your thoughts on this work.
Elsewhere in the archive
Join the Discussion
Join the discussion
Sign in to leave a comment or review.
Sign InorCreate an account