One of the principal reasons of durability in asphalte pavement is its
elasticity, and it should be remembered that compressed asphalte does
not begin to “wear” until all compression has ceased; this is the case
with no other system of pavement--stone and wood both begin “wearing”
from the day the traffic commences. Under ordinarily heavy traffic it
may be estimated that it will take two years to complete the compression
of asphalte, and the weight of a square foot of this pavement will at
the expiration of that time be nearly the same as on the day it was
laid, though the thickness is reduced during the first two years as
much as it will be in the following eight.
Much is said about the advisability of _good_ and _dry_ concrete, but it
may be as well to explain the reasons that necessitate so much care in
the foundation. First, it should be always borne in mind that asphalte
pavement is nothing more than a tough “carpet,” and has no power of
itself of offering resistance to heavy traffic; consequently, if the
substratum or concrete is not thoroughly solid and resisting, the weight
of traffic will crush it, and the asphalte will at once give way in all
directions. The concrete should be made strong enough to resist the
traffic, and the asphalte is a simple covering to protect the concrete
from direct contact with the wear and friction caused by the traffic. So
much for the strength, but the dryness is of even still greater
importance; for the best asphalte, laid by skilled workmen, on
thoroughly first-rate but damp concrete, will rapidly go to pieces--a
phenomenon takes place, which, although quite natural, is little
realised by most engineers. When the hot asphalte is laid, the water is
immediately sucked up and turned into steam, which tries to escape
through the heated powder, and the result is that although the surface
of the asphalte is smooth, the mass is really disintegrated from
underneath by its bitter enemy “water,” and as soon as the surface
begins to wear, the fissures formed by the passing of the steam appear
on the surface and the whole pavement falls to pieces: thus accounting
for some of the failures this description of roadway has met with under
unskilled treatment.
This completes the subject of roadways; I will turn to that of footpaths
in the next chapter.
[90] In this respect the Seyssel is the best, being of a very fine
grain.
[91] _Vide_ ‘Minutes of Proceedings of Institution of Civil
Engineers,’ vol. lx.
[92] _Vide_ Mr. Howarth’s paper on ‘Wood as a Paving Material under
Heavy Traffic,’ ‘Minutes of Proceedings of the Institution of Civil
Engineers, vol. lviii. p. 35.
[93] In Paris and other cities liable to civil war or internal
commotions, it is contended as an advantage of asphalte that it cannot
be used for the construction of barricades, breastworks, or rifle
pits.
Public-domain text, read in full here on John Shaqi.
Reviews
Reviews
No reviews yet
Be the first to share your thoughts on this work.
Elsewhere in the archive
Join the Discussion
Join the discussion
Sign in to leave a comment or review.
Sign InorCreate an account