=235. Weighing the Copper as Oxid.=—In the usual methods of the
determination of reducing bodies, the percentage is calculated either
volumetrically from the quantity of the sugar solution required to
decolorize a given volume of the alkaline copper solution, or the
reduced copper suboxid is brought into a metallic state by heating in
an atmosphere of hydrogen or by electrolytic deposition. A quicker
method of procedure is found in completing the oxidation of the cupric
oxid by heating to low redness in a current of air.[192] For this
determination the precipitation of the cuprous oxid and its filtration
are made in the usual manner. The cuprous oxid is collected in a
filtering tube, made by drawing out to proper dimensions a piece of
combustion tube, and has a length of about twelve centimeters in all.
The unchanged part of the tube is about eight centimeters in length
and twelve millimeters in diameter. It is filled by first putting in
a plug of glass wool and covering this with an asbestos felt on top
of which another plug of glass wool is placed. After the cuprous oxid
is collected in the tube it is washed with boiling water, alcohol and
ether. The rubber tube connecting it with the suction is of sufficient
length to permit the tube being taken in one hand and brought into
a horizontal position over a bunsen. The tube is gradually heated,
rotating it meanwhile, until any residual moisture, alcohol or ether,
is driven off from the filtering material. The layer of glass wool
holding the cuprous oxid is gradually brought into the flame and as
the oxidation begins the material will be seen to glow. The heating is
continued for some time after the glowing has ceased, in all for three
or four minutes, the tube and the copper oxid which it contains being
brought to a low redness. The current of air passing over the red-hot
material in this time oxidizes it completely. The filtering tube,
before use, must be ignited and weighed in exactly the same manner as
described above. The heat is so applied as not to endanger the rubber
tube attached to one end of the filtering tube nor to burn the fingers
of the operator as he turns the tube during the heating. After complete
oxidation the tube is cooled in a desiccator and weighed, the increase
of weight giving the copper oxid. For the atomic weights, 63.3 copper
and 15.96 oxygen, one gram of copper oxid is equivalent to 0.79864
gram of copper, and for the weights 63.17 copper and 15.96 oxygen, one
gram of copper oxid equals 0.79831 gram of copper. From the amount of
metallic copper calculated by one of these factors, the reducing sugar
is determined by the tables already given.
Public-domain text, read in full here on John Shaqi.
Reviews
Reviews
No reviews yet
Be the first to share your thoughts on this work.
Elsewhere in the archive
Join the Discussion
Join the discussion
Sign in to leave a comment or review.
Sign InorCreate an account