"Take 100 to 1000 grains and attack with aqua regia in a flask; cool
for about thirty minutes or more; dilute with water and filter. If
gold is present, it will now be held in solution in the filtrate.
Remove the filter and evaporate the filtrates to dryness; then add a
little hydrochloric acid, evaporate and re-dissolve the dry salt in
warm water; add to the solution so formed proto-sulphate of iron;
which will throw down the gold in the form of a fine, dark
precipitate. The precipitate is seldom fine, being mixed with oxides
of iron, and must now be dried in the filter paper, and both burned
over the lamp in a porcelain dish. Then mix the dried precipitate with
three times its weight of lead; fuse, scorify and cupel. In case
platinum, iridium, etc., are found associated with the gold, an extra
amount of fine silver should be added before cupellation, and the gold
button will be found pure."
In one of his reports the State Mineralogist of California gives a
most lucid description of a mechanical assay of gold-bearing sands,
stamped ore, etc., etc. He states:
"It must be understood that this is only a working test. It does not
give all the gold in the rock, as shown by a careful fire assay, but
what is of equal importance to the mine-owner, mill-man, and practical
miner, it gives what he can reasonably expect to save in a good quartz
mill. It is really milling on a small scale. It is generally very
correct and reliable, if a quantity of material be sampled. The only
operation which requires much skill is the washing, generally well
understood by those who are most likely to avail themselves of the
instructions. These rules apply equally to placer gravels. Take a
quantity of the ore--the larger the better--and break it into
egg-sized pieces. Spread on a good floor, and with a shovel mix very
thoroughly; then shovel into three piles, placing one shovelful upon
each in succession until all is disposed of. Two of the piles may then
be put into bags. The remaining pile is spread on the floor, mixed as
before, and shovelled in the same manner into three piles. This is
repeated according to the quantity sampled, until the last pile does
not contain more than 30 pounds of ore. As the quantity on the floor
becomes smaller, the lumps must be broken finer until at last they
should not exceed one inch in diameter. The remainder is reduced by a
hammer and iron ring to the size of peas. The whole 30 pounds is then
spread out, and after careful mixing portions are lifted with a flat
knife, taking up the fine dust with the larger fragments, until about
10 pounds have been gathered. This quantity is then ground down fine
with the muller, and passed through a 40-mesh sieve. If the rock is
rich, the last portion will be found to contain some free gold in
flattened discs, which will not pass this sieve. These must be placed
with the pulverized ore, and the whole thoroughly mixed, if the
quantity is small, but if large must be treated separately, and the
Public-domain text, read in full here on John Shaqi.
Reviews
Reviews
No reviews yet
Be the first to share your thoughts on this work.
Join the Discussion
Join the discussion
Sign in to leave a comment or review.
Sign InorCreate an account