It must not be imagined that this preparation for work is not very
important. I am convinced that less depends on the quality of the ink
than on a surface freed from all acid and mucous substances and provided
with a sufficient amount of fat.
On the stone thus prepared the rough design may be done with lead crayon
or red chalk or by tracings or transfers. Any surplus of lead or red
chalk would make trouble during the succeeding completion of the design
with chemical ink, and must be removed carefully. If the design has
been laid on by transfer, the resultant fattiness must be lightly rubbed
away with a fine sand, but not so as to injure the design.
This method, of first drafting the design on paper with soft chemical
transfer ink and then transferring to stone, offers such advantages that
it pays to practice it. Care must be taken to remove all surplus of
color, as otherwise all lines that should not appear will resist the
etching fluid and gradually show again. Those who fear destruction of
the design by the use of sand can effect the same purpose by printing
off on clean waste paper a few times, or the design may be printed off
on paper before being transferred, thus cleansing it of surplus fat.
When the design has been laid on the stone clean and strongly with
chemical ink, the plate can be etched and prepared, but not till the
whole design is perfectly dry, because otherwise it cannot resist the
action of the fluid.
The parts finished first usually are dry long before the entire work is
finished. A trained eye can recognize the proper degree of dryness from
the sheen, which varies with different kinds of ink, but on the whole is
always duller when the design is dry than while it still is wet. It is
highly necessary that the design be thoroughly dry. It is possible to
keep a designed plate for years without etching it, so long as it is
protected against injury.
Etching is done in two ways, painting the fluid on and pouring it on.
The former method is less circumstantial, but is used only in coarser
work, because there is always danger of damaging delicate parts of the
design. It has the advantage, however, that any dirt caused by
corrections will be removed. A mixture of three or four parts of water
with one part of aquafortis is painted over the stone with a soft brush
of fox- or badger-hair. The brush must be dipped continually because the
fluid loses its power.
For the second method the stone is placed in a large wooden trough or
box, provided with cross-pieces to keep the stone from the bottom. The
acid, thinned down with thirty or forty parts of water, is poured over
it. It is rather immaterial how much one may dilute the acid. Very weak
solutions simply mean that the pouring must be repeated oftener. The
fluid acts on stones according to their degree of hardness. Regard must
be had, too, to the delicacy of the design, very fine lines being unable
to resist etching that does not affect coarse lines.
Public-domain text, read in full here on John Shaqi.
Reviews
Reviews
No reviews yet
Be the first to share your thoughts on this work.
Elsewhere in the archive
Join the Discussion
Join the discussion
Sign in to leave a comment or review.
Sign InorCreate an account