Lead Smelting and Refining, With Some Notes on Lead Mining
Science
Lead Smelting and Refining, With Some Notes on Lead Mining
Lead -- Metallurgy; Lead mines and mining
At the smelting plant of the Tennessee Copper Company we have lately
installed blast-furnace piston-blowing engines; the steam cylinders
are of the Corliss type and are 13 and 24 in. by 42 in.; the blowing
cylinders are two in number, each 57 × 42 in.; the air valves are all
Corliss in type. These blowing engines are designed to operate at a
maximum air pressure of 2½ lb. per square inch.
At the Santa Fe Gold and Copper Mining Company’s smelter we have
recently installed a No. 8 blower directly coupled to a 14 × 32 in.
Corliss engine. This blower has been in use about five months and is
giving very good results against the comparatively low pressure of 12
oz., or ¾ lb.
During the coming summer it is my intention to make careful volumetric
and horse-power tests on these two types of machines under similar
conditions of air pressure, and to publish the results; but in the
meantime I wish to correct the error that a rotary blower of the
impeller type is not a practicable machine at pressure over 5 lb.
BLOWERS AND BLOWING ENGINES FOR LEAD AND COPPER SMELTING
BY HIRAM W. HIXON
(July 20, 1901)
In the _Engineering and Mining Journal_ for July 6th I note the
discussion over the relative merits of blowers and blowing engines for
lead and copper smelting, and wish to state that, irrespective of the
work to be done, the blast pressure will depend entirely on the charge
burden in any kind of blast-furnace work, and that the charge burden
governs the reducing action of the furnace altogether. Along these
lines the iron industry has raised the charge burden up to 100 ft. to
secure the full benefit of the reducing action of the carbon monoxide
on the ore.
In direct opposition to this we have what is known as pyritic smelting,
wherein the charge burden governs the grade of the matte produced to
such an extent that if a charge run with 4 to 6 ft. of burden above the
tuyeres, producing 40 per cent. matte, is changed to a charge burden of
10 or 12 ft., the grade of the matte will decrease from 40 per cent. to
probably less than 20 per cent. I can state this as a fact from recent
experience in operating a blast furnace on heap-roasted ores under the
conditions named, with the result as above stated.
Public-domain text, read in full here on John Shaqi.
Reviews
Reviews
No reviews yet
Be the first to share your thoughts on this work.
Elsewhere in the archive
Join the Discussion
Join the discussion
Sign in to leave a comment or review.
Sign InorCreate an account