Silver. Silver ore may be detected by dissolving a small quantity in a
test tube with a few drops of nitric acid. Boil until all the red
fumes disappear. Let the solution cool, and add a little water. Filter
the whole, and add a few drops of muriatic acid, which will
precipitate the white chloride of silver. Dissolve this precipitate
with ammonia; then add nitric acid once more. Exposed to the light,
the precipitate soon shows a violet tint. Pure silver is the brightest
of metals, of a brilliant white hue, with rich luster. To detect
chloride of silver in a pulp, rub harshly with a clean, bright and wet
copper cartridge or coin, and if there be silver in the pulp the
copper will be coated with it. Graphite will also whiten copper, but
the film is easily rubbed off.
Nickel. Nickel may be determined as follows: A little of the powdered
ore taken up on the point of a penknife, and dissolved in a mixture of
ten drops of nitric and five drops of muriatic acid, should be boiled
over a lamp for a few minutes, and ten or twelve drops of water added.
A small quantity of ferrocyanide of potash will throw down a
whitish-green precipitate, indicating nickel.
Platinum. Platinum is a most refractory metal to treat, as it must be
boiled for at least two hours in the mixture of muriatic and nitric
acid, known as aqua regia. A small amount of alcohol is to be added to
the solution, and the latter filtered. The platinum is precipitated
with ammonia chloride.
Manganese. Manganese may be proved as follows: A few grains of
powdered ore are placed in a test-tube, with three or four drops of
sulphuric acid. Two or three grains of granulated lead or litharge
being dropped in, the color will become pink should manganese be in
the ore.
A preliminary examination of a mineral may be made with a pocket lens
and a penknife. With the first, any conspicuous constituents may be
recognized, while a scratch with the point of the latter will give an
idea as to the softness or hardness of the mineral. Should much quartz
(silica) be present, a sharp blow with the steel will cause sparks.
The next test should be with some ore powdered and held over a spirit
flame. A drop or two of water and a drop of sulpho-cyanide of potash
will reveal iron, should such be present, by a deep red coloration.
To another portion add one drop of hydrochloric acid, and a dense,
curdy precipitate will indicate silver, if there be any.
Added to the same original nitric acid solution, several drops of
ammonia water would detect copper by a blue color.
Antimony, tin, aluminum, zinc, cobalt and nickel, uranium and titanium
are best shown by the blowpipe.
Public-domain text, read in full here on John Shaqi.
Reviews
Reviews
No reviews yet
Be the first to share your thoughts on this work.
Join the Discussion
Join the discussion
Sign in to leave a comment or review.
Sign InorCreate an account